Description


Grade

U.K.

Germany

U.S.A.

Russia

Standard

 

Hiperco 50A

AFK502

Permendur

Vacoflux 50

Supermendur HiperCo50


GB/T15002-1994

Chemical Composition (%)

C

Mn

Si

P

S

Cu

Ni

Co

V

Fe




0.04

0.30

0.30

0.020

0.020

0.20

0.50

49.0~51.0

0.80~1.80

Balance











 

 

Table 3 DC Magnetic Property Requirements After Heat-Treated

Type

Minimum Magnetic Flux Density for Different Magnetic Field Strengths (T)

Coercive force

Hc / (A/m)≤

B400

B800

B1600

B2400

B4000

B8000


Cold rolled Strips

1.70

1.90

2.00

2.10

2.20

2.25

110

Wires,Forgings,Billets,Bars

1.60

1.70

1.80

2.05

2.15

2.20

144

 

 

 Physical Property


Resistivity /(μΩ•m)

Density/(g/cm3)

Curie point/°C

Magnetostriction Cofficient/(×10-6)

Tensile Strength,N/mm2

Unannealed

Annealed

0.40

8.20

980

60~100

1325

490

 Applications

Electrical generators, pole pieces for electromagnets, magnetic bearings and high magnetic flux devices and instruments.


Forms available

Forged bar, hot-rolled bar, cold-drawn bar, cold-rolled strip.