Description

Chemical composition

Alloy

%

Ni

Cr

Fe

C

Mn

Si

Cu

Al

Ti

Co

GH90

Min.

Bal

18






1.0

2

15

Max.

21

1.5

0.13

1.0

1

0.2

2.0

3

21

Mechanical properties

Alloy status

Tensile strength
Rm N/mm²

Yield strength
R P 0.2N/mm²

Elongation
A 5 %

Modulus of Rigidity

Density
g/cm³

Melting Point

°C

Annealing
treatment

800-1000



82.5kN/mm2

8.2

1370

Heat treatment

Supplied in alloy wire

Type

Temperature°C

Time(Hr)

Cooling

Spring temper

Age harden

650

4

Air

Spring temper

Age harden

600

16

Air

Annealed

Age harden

750

4

Air

Supplied in plate or strip

Age harden

700-725

4

Air






 

 

Features:

1,High stress rupture strength and high creep resistance at high temperatures.

2,Good resistance to high-temperature corrosion and oxidation.

3,Age-hardenable.

4,High temperature dynamic applications.

 

Applications:

The alloy is used for turbine blades, discs, forgings, ring sections and hot-working tools. Also used to make Aerospace fasteners.

 

Standard

AMS 5829 

GH4090

W.Nr. 2.4632

UNS NO7090

AWS 030

 

 

Forms Available

Plate, sheet, strip, bar, wire, rod, pipe, tube, forging.
FAQ:

Q:What is your working time?

A;Monday-Saturday : 7:30AM-17:00PM (Beijing time, GMT+08.00) We have public holiday during May.1-3, Oct.1-7 and Chinese New Year holiday . Pls email us during our holiday if u have any question.

Q:Do you provide free samples?

A:Yes, we can provide a free sample for testing,buyer should bear all the shipping costs.

Q:What is your payment terms?

A:T/T,L/C,D/A,D/P,Western Union,MoneyGram,Paypal What is the lead time? Usually sample lead time is 7 days after payment has been confirmed.

Packaging Details:

Wire is packed with waterproof paper or weave bag, into pallets or wooden case.Special packaging requirements can also be accommodated.